CNC machining materials, and what the same part costs in each
We machine ten grades: aluminum 6061-T6 and 7075-T6, copper C110, brass C360, steel 1018 and 4140 prehard, stainless 304 and 316, titanium grade 5, and acetal (Delrin). Below is what each is for, how it cuts, which finishes it takes, what the stock costs, and what one test bracket and one test shaft cost in each, worked out from the same price list as our instant quote.
The same part in ten materials
These are two of the test parts we check our quote engine against, not customers’: a bracket, 80 × 60 × 18 mm, milled from the top and the bottom with one tapped M5 hole and two counterbored ones, and a shaft, Ø40 mm at its widest and 75 mm long, turned on the lathe with a Ø10 mm hole in one end. Ten of each, at standard tolerance, 10 business days, as machined. Prices are in Canadian dollars, before tax and shipping.
| Material | Stock, a kg | Roughing, cm³ a minute | Bracket, each | Shaft, each |
|---|---|---|---|---|
Prices load from the live price list.Upload a model | ||||
“Roughing” is the rate our quote plans on for taking the bulk of the stock off. It’s an estimating number, not a feed or speed, and it’s the plainest way to see how a material cuts: the lower it is, the longer the part is on the machine.
Read down the table and the price follows the cutting rate more than the stock price. The bracket’s material charge is in 6061 and in 304, but ten brackets cost each in 6061 and in 304. The difference is time on the machine.
How the material is priced
The quote prices the stock your part is cut from, not the part’s own weight:
- A milled part is cut from a block 3 mm bigger than the part on every side. The bracket’s block is 86 × 66 × 24 mm.
- A turned part is cut from round bar 3 mm bigger a side: the Ø40 × 75 mm shaft comes from Ø46 × 81 mm bar.
- The charge is the stock’s weight times the price a kilogram in the table, plus 15% for cutting, freight and waste.
- Each part carries a minimum material charge of .
For the bracket: its block weighs kg in 6061, which works out to , so it pays the minimum. In C110 copper the same block weighs kg and the charge is . In titanium grade 5 it weighs kg and the charge is .
So on a small part in aluminum, steel or acetal, the grade’s price a kilogram hardly shows. On a part cut from a big block of copper, stainless or titanium, it does. The instant quote’s price breakdown shows the material on its own line.
Aluminum: 6061-T6 or 7075-T6
6061-T6 is the default for a machined part: brackets, housings, fixture plates, manifold blocks and cold plate blanks. It’s the fastest-cutting metal on our list; the quote plans on roughing 40 cm³ a minute. Stock is a kilogram.
7075-T6 is the stronger alloy, for a part that carries more load for its size. It cuts almost as fast (35 cm³ a minute), and stock is a kilogram. On a small part the upgrade costs little: ten test brackets are more in 7075 than in 6061, because both pay the minimum material charge. One thing to design for: 7075 plate holds stress, and floors or walls under 1.5 mm can bow 0.1 to 0.5 mm once they’re cut free. Keep them thicker, or we stress relieve and finish in two passes.
- Finishes for both: bead blast, type II anodize, hard type III anodize, powder coat.
- Limits: walls get a second look under 0.8 mm and need changing under 0.5 mm. A tapped hole needs 1.5 × the thread diameter, 9 mm for an M6.
Where a part is in 7075 and may not need it, the quote in your dashboard suggests 6061 and shows what it saves.
Stainless steel: 304 or 316
304 is the general stainless grade: flanges, adapters, vacuum hardware and mounts. 316 is the one to pick where the part meets salt or chemicals: valve components and fittings.
Both cut slowly. The quote plans on roughing 7 cm³ a minute in 304 and 6 in 316, against 40 in 6061, and on tapping a hole taking twice as long as in aluminum. Stock is a kilogram for 304 and for 316. Ten test brackets cost more in 316 than in 304.
- Finishes for both: bead blast, passivate, powder coat.
- Limits: walls get a second look under 1.0 mm and need changing under 0.6 mm. A tapped hole needs 1.2 × the thread diameter, 7.2 mm for an M6.
- Galling: stainless screws in stainless threads cold weld when tightened dry. Use anti-seize, or a screw of a different material or hardness.
Steel: 1018 or 4140 prehard
1018 is plain low-carbon steel, for fixtures, spacers, shafts and flanges that don’t need to resist corrosion or wear. It has the cheapest stock on our list, a kilogram, and the quote plans on roughing 12 cm³ a minute.
4140 prehard is alloy steel that arrives already hardened, for tool components and shafts that take load or wear. It cuts slower (8 cm³ a minute), and the quote allows 1.6 times as long for each hole. Stock is a kilogram. Ten test brackets cost more in 4140 than in 1018.
- Finishes for both: bead blast, black oxide, powder coat.
- Limits: walls get a second look under 0.8 mm and need changing under 0.5 mm. A tapped hole needs 1.2 × the thread diameter, 7.2 mm for an M6.
Copper C110 and brass C360
C110 copper is for carrying current and heat: busbar, switchgear hardware and cold plates. It’s heavy and its stock costs more than most, a kilogram, so the material charge shows even on a small part, and the quote plans on roughing 12 cm³ a minute.
C360 brass is the fast-cutting one of the two (30 cm³ a minute, close to aluminum), for fittings, adapters and valve components. Stock is a kilogram.
- Finishes for both: bead blast, tin plate, powder coat.
- Limits: walls get a second look under 0.8 mm and need changing under 0.5 mm. A tapped hole needs 1.6 × the thread diameter, 9.6 mm for an M6.
Titanium grade 5
Grade 5 (Ti-6Al-4V) is for parts that must be strong and light, or stand up to corrosion: lab and vacuum hardware and weight-critical brackets. It is the slowest and dearest material on our list. The quote plans on roughing 3 cm³ a minute, against 40 in 6061, and stock is a kilogram. Ten test brackets are each in titanium, against in 6061.
- Finishes: bead blast, powder coat. Anodizing is offered on aluminum only.
- Limits: walls get a second look under 1.0 mm and need changing under 0.6 mm. A tapped hole needs 1.2 × the thread diameter, 7.2 mm for an M6.
Before you pick it, price the part in 316 or 7075 as well. The instant quote changes as you switch material.
Acetal (Delrin)
Acetal is the one plastic on our list: gripper fingers, fixtures, bushings and insulating parts. It cuts faster than anything else we machine (50 cm³ a minute), and it’s light, so a small part pays the minimum material charge. Stock is a kilogram.
- Finishes: as machined only. Bead blast and powder coat aren’t offered on plastics.
- Limits: walls get a second look under 1.5 mm and need changing under 1.0 mm. A tapped hole needs 2.5 × the thread diameter, 15 mm for an M6, so ask for threaded inserts where the part is thin.
Finishes by material
Each finish has a lot charge, paid once an order for that finish whatever the quantity, a charge a part, and the business days it adds. The last column is what it adds to ten test brackets.
| Finish | Lot | A part | Days added | On ten brackets |
|---|---|---|---|---|
| Prices load from the live price list. | ||||
On one part the lot charge is nearly the whole cost of a finish. Parts on the same order with the same finish share one lot charge.
Wall and thread limits by material
The design checks run on every model as you add it. These two change with the material; the rest are in our design guidelines.
| Material | Walls: look at under, change under | Thread engagement, for an M6 |
|---|---|---|
| Aluminum | 0.8, 0.5 mm | 1.5 ×, 9.0 mm |
| Steel | 0.8, 0.5 mm | 1.2 ×, 7.2 mm |
| Brass, copper | 0.8, 0.5 mm | 1.6 ×, 9.6 mm |
| Stainless, titanium | 1.0, 0.6 mm | 1.2 ×, 7.2 mm |
| Acetal | 1.5, 1.0 mm | 2.5 ×, 15 mm |
Thread engagement is the length of thread a tapped hole needs, as a multiple of the thread’s diameter. See wall thickness and thread depth for how to fix each.
Material certs
Material certs are a paid add-on: a part line. Add them on the quote when your job needs them. A CMM inspection report and a first article report are paid add-ons too; what each costs is on CNC machining cost.
Questions
What is the best aluminum for machining?
For most parts, 6061-T6. It cuts fastest, its stock costs less than 7075’s, and it takes both kinds of anodize. Pick 7075-T6 when the part needs the strength, and keep its floors and walls 1.5 mm or thicker.
How machinable is 316 stainless steel?
It’s the slowest stainless on our list. Our quote plans on roughing it at about a seventh of the rate of 6061 aluminum, and 304 is a little quicker. If the part doesn’t meet salt or chemicals, 304 costs less. We don’t list a free-machining stainless grade.
Is titanium hard to machine?
It’s the slowest material we cut and its stock costs the most, so our test bracket costs about three times as much in titanium as in 6061. Our grade is grade 5, Ti-6Al-4V. Price the part in 316 or 7075 as well before you settle on it.
Can you make anodized aluminum parts?
Yes. Type II and hard type III anodize are offered on 6061 and 7075. Each has a lot charge paid once an order, a charge a part, and adds business days: type II is for the lot, a part and 4 days.
What is the best plastic for machining?
Acetal (Delrin) is the one plastic on our list. It cuts faster than any metal we machine and holds its size well. Keep walls 1.5 mm or thicker and give threads 2.5 × their diameter, or ask for threaded inserts.
Do you machine aluminum bronze, Inconel or magnesium?
They aren’t on our price list, so the instant quote can’t price them. Ask us: email quotes@highlandmetal.ca, or put it in the notes for the machinist when you send a request, and we’ll tell you whether it can be made.
Upload a model and see the price in Canadian dollars, or book a call and talk it through with a machinist.